molybdenum (sintered/ arc cast) refractory alloys material property data sheet

Search:


Metal Suppliers Online: Material Property Data

Refractory Alloys Molybdenum (Sintered/ Arc Cast)

 


Specifications

The following specifications cover Refractory Alloys Molybdenum (Sintered/ Arc Cast)

 

 


Property Results

No Related Metal names.


Chemistry Data : [top]

There is no chemistry data available for this grade.


Principal Design Features Molybdenum is a metallic element, like iron or aluminum. While most commonly employed as an alloying element, it is also used in its pure form. It possesses excellent high temperature strength, has a very high melting point (4730 F) and is a good thermal and electrical conductor. Additionally, moly has a relatively low coefficient of thermal expansion.

Applications Moly is commonly employed in high temperature applications such as heating elements in furnaces, filament supports in electric lamps, heat shields and in hearth trays, plates and racks.

Machinability Machinists describe machining moly as similar to machining cast iron. High speed or carbide tools have been successfully employed with a general preference towards carbide. Moly is a very abrasive material and rigid set-ups and sharp tools are key. The alloy can have a tendency to "tear" if positive feeds are not used.

Forming Moly can be successfully formed, but a word of caution is recommended. The material will form most efficiently when bending transverse or against its grain or rolling direction. Cracking is a common and costly problem. Heating the workpiece prior to forming can minimize these problems

Welding Welding moly can best be performed in an argon or helium atmosphere. Best welds are obtained using electron beam methods. Resistance methods are possible, however the resulting weld "nuggets" will be hard and brittle and the weld itself will not be as strong as could be obtained with EB.

Annealing Recrystallization temperature is dependent upon prior working and condition, however the average required temp is in the range of 2100 F. Stress relieving temperature is 1600 - 1800 F.

Physical Data : [top]

Density (lb / cu. in.) 0.37
Electrical Resistivity (microhm-cm (at 68 Deg F)) 31
Melting Point (Deg F) 4730
Thermal Conductivity 84.5
Mean Coeff Thermal Expansion 2.8


Mechanical Data : [top]

There is no Mechnical data available for this grade.


[top]
Nickel - www.nidi.org

Copper - www.copper.org

Titanium - www.titanium.org

Steel Lynx - www.mlc.lib.mi.us/~stewarca/steelynx.html


Disclaimer
This information is provided "as is" and Metal Suppliers Online, Inc. makes no warranty of any kind with respect to the subject matter or accuracy of the information contained herein. Metal Suppliers Online, Inc. specifically disclaims all warranties, expressed, implied or otherwise, including without limitation, all warranties of merchantability and fitness for a particular purpose.

In no event shall Metal Suppliers Online, Inc. be liable for any special, incidental, indirect or consequential damages of any kind or any damages whatsoever resulting from loss of use, data, profits, whether or not advised of the possibility of damage, and on any theory of liability, arising out of or in connection with the use of the information contained herein.

This publication may include technical inaccuracies or typographical errors. Changes may be periodically made to the information herein.


Use of this Web Site constitutes acceptance of the Metal Suppliers Online User Agreement.
Copyright © 1995-2024 Metal Suppliers Online, LLC. All Rights Reserved.
Metal Suppliers Online Privacy Policy  |  Contact Us